Publication date: 29 June 2012

Manzoor Ahmad, J. Luo, Ben Xu, Hendra Purnawali, Peter King, Paul Chalker, Yongqing Fu, Weimin Huang and Moshen Miraftab

Shape memory polyurethanes (SMPUs) are typically synthesized using polyols of low molecular weight, Mw, and high hydroxyl number as it is believed that high density of cross-links…

50

Abstract

Shape memory polyurethanes (SMPUs) are typically synthesized using polyols of low molecular weight, Mw, and high hydroxyl number as it is believed that high density of cross-links in these polyols are essential for high performance shape memory polymers. In this study, polyethylene glycol (PEG-6000) with Mw ~ 6000 g/mol and low hydroxyl number (OH ~ 18 mg K OH/g) as the soft segment and diisocyanate as the hard segment were used to synthesize SMPUs. It revealed that although the PEG-6000 based SMPUs have lower maximum elongation at break (425%) and recovery stress than those of PCL-2000 polyol based SMPUs, they have much better shape recovery ratio (98%) and shape fixity (95%). Furthermore, these SMPUs showed a much shorter actuation time of <10sec for up to 85% shape recovery, much shorter than those low Mw SMPUs, clearly demonstrated their great potential for applications.

Details

World Journal of Engineering, vol. 9 no. 3
Type: Research Article
ISSN: 1708-5284

Keywords

1 – 1 of 1
Per page
102050