Summary of major factors affecting mechanical properties of TiZr based alloys
Abstract
Effects of major factors, such as alloy composition, crystal structure and grain size, on mechanical properties of TiZr based alloys are investigated and summarized in this work. The microhardness of TC4 alloy obviously increases 15.3% and 17.6% after 30 wt.% and 47 wt.% Zr additions, respectively. Nanoindentation results show that the average nanoindentation hardness of α phase in annealed 30 Zr is approximately 18% higher than that of retained β phase. Tensile test results show that variation in strength of basketweave microstructural 30 Zr alloy with original β grain size from 100 to 203 μm is less than 2%.
Keywords
Citation
Yin, L., Liang, S. and Zheng, L. (2015), "Summary of major factors affecting mechanical properties of TiZr based alloys", World Journal of Engineering, Vol. 12 No. 4, pp. 319-324. https://doi.org/10.1260/1708-5284.12.4.319