Photoelastic Measurement of Surface Strain: Investigation of a Direct Method Using an Optically Sensitive Material Bonded to the Metal Component

Aircraft Engineering and Aerospace Technology

ISSN: 0002-2667

Article publication date: 1 September 1960

18

Abstract

Tapered and Parallel Shank Specimens Tapered and parallel shank specimens were loaded in increments of 200 lb. up to about 1,300 lb., generally the maximum for both types.

Citation

Linge, J.R. (1960), "Photoelastic Measurement of Surface Strain: Investigation of a Direct Method Using an Optically Sensitive Material Bonded to the Metal Component", Aircraft Engineering and Aerospace Technology, Vol. 32 No. 9, pp. 261-270. https://doi.org/10.1108/eb033298